Synthesis of Zn2TiO4 via solidstate method as a promising additive for ...
The composite was milled for 1 h using a planetary ball mill () by first milling for 15 min, resting for 2 min and milling for another 15 min in a different direction for 2 cycles at the rate of 400 rpm. The weight of the balltopowder ratio was 40:1. ... L = mean size of the crystallite. K = Scherer constant.